中国电力 ›› 2014, Vol. 47 ›› Issue (4): 5-8.DOI: 10.11930/j.issn.1004-9649.2014.4.5.3

• 专稿 • 上一篇    下一篇

超超临界锅炉高温再热器T91/HR3C异种钢接头失效分析

王伟1, 王学2, 钟万里1, 胡磊2, 胡平1   

  1. 1. 广东电网公司 电力科学研究院,广东 广州 510080;
    2. 武汉大学 动力与机械学院,湖北 武汉 430072
  • 收稿日期:2014-01-03 出版日期:2014-04-30 发布日期:2015-12-22
  • 作者简介:王伟(1983-),男,河南灵宝人,博士,高级工程师,从事电厂和电网金属材料的理化检验、失效分析及技术监督等。E-mail: wwangcn@163.com
  • 基金资助:
    南方电网公司科技资助项目(K-GD2012-388)

Failure Analysis of T91/HR3C Dissimilar Steel Welded Joints in High-Temperature Reheater of USC Boilers

WANG Wei1, WANG Xue2, ZHONG Wan-li1, HU Lei2, HU Ping1   

  1. 1. Electric Power Research Institute of Guangdong Power Grid Corporation, Guangzhou 510080, China
    2. School of Power and Mechanics, Wuhan University, Wuhan 430072, China
  • Received:2014-01-03 Online:2014-04-30 Published:2015-12-22
  • Supported by:
    This work is supported by Science and Technology Project of China Southern Power Grid Company Limited (K-GD2012-388)

摘要: 在超超临界火电机组锅炉受热面管的高温段有许多异种钢接头,其焊接质量及性能直接影响机组的安全运行。对某3 033 t/h超超临界锅炉高温再热器T91/HR3C异种钢接头的失效试样进行了宏/微观分析。研究表明,失效部位在T91侧热影响区,裂纹沿管子周向分布,从外壁粗晶粒热影响区启裂,终止于细晶粒热影响区。焊后热处理不充分,T91侧热影响区组织不稳定和硬度高是异种钢接头失效的主要原因,建议再次进行焊后热处理以改善接头性能和消除焊接应力。此外,研究发现T91侧熔合线附近形成白亮的低硬度δ-铁素体,其对接头失效虽无直接影响,但对接头长期性能的影响需要进一步评估。

关键词: T91钢, HR3C钢, 异种钢焊接, δ, -铁素体, 电站锅炉

Abstract: Many dissimilar steel joints are used in the high-temperature section of boiler heating surface tubes of ultra-supercritical (USC) thermal power units and their welding quality and performance directly determines the operation security of the units. Macroscopic and microscopic examinations on the failure specimen of T91/HR3C dissimilar steel welded joints are conducted for the high-temperature reheater in a 3 033-t/h USC boiler. The results show that the failure part is located in the heat affected zone of T91 side with the cracks spreading along the circumferential direction of the tubes, starting from the CGHAZ and ending at the FGHAZ of the outer wall. The insufficient post-welding heat treatment, unstable microstructure in the HAZ and high hardness are the major causes leading to the cracking failure. Post-welding heat treatment(PWHT) is suggested to improve the ductility and reduce the residual stress for the welded joints. Furthermore, the delta ferrite of lower hardness white and bright is observed near the fusion line of T91 side. It is not directly related to the failure, but further study is required to evaluate its influence on the long-term performance of the welded joints.

Key words: T91 steel, HR3C steel, dissimilar steel welding, delta ferrite, utility boiler